| Project: |
Guggenheim Museum |
| Location: |
Bilbao, Spain |
| Architect: |
Frank O. Gehry & Associates - Santa Monica, California |
| Material: |
TIMETAL® 35A Commercially Pure Grade 1 Titanium, 0.016" thick |
| Application: |
42,875 interlocking 24" x 48" flat seam panels, annealed and pickled finish. A total of 343,000 ft2 cover the Museum's exterior. |
|