Comparison of physical properties with those of other metals

ItemAtomic No.Atomic wt.Specific
gravity
Melting
point
(°C)
Linear thermal
expansion
coefficient
(/°C)
Specific
heat
(cal/gr/°C)
Thermal conductivity
coefficient
(cal/cm2/sec/°C/cm)
Specific
electrical
resistance
(µOhm-cm)
Electrical
conductivity
(%IACA)
Young's
modulus
(kg/mm2)
Poisson's
ratio
Titanium2247.904.51,5688.4X10-60.1240.041553.110,8500.34
18-8 Stainless
steel (SUS 304)
--------7.91,400
~1,420
17X10-60.120.039722.420.4030.3
Aluminum1326.972.766023X10-60.210.492.7647,0500.33
Magnesium1224.321.765025X10-60.240.384.3404,5700.35
Nickel2858.698.91,45315X10-60.110.229.51821,0000.30
Copper2963.578.91,08317X10-60.0920.921,72410011,0000.34