FOREWORD
Since titanium metal first became a commercial reality in 1950, corrosion resistance has been an
important consideration in its selection as an engineering structural material. Titanium has gained
acceptance in many media where its corrosion resistance and engineering properties have provided
the corrosion and design engineer with a reliable and economic material.
This brochure summarizes the corrosion resistance data accumulated in over forty years laboratory
testing and application experience. The corrosion data were obtained using generally acceptable
testing methods; however, since service conditions may be dissimilar, TIMET recommends testing
under the actual anticipated operating conditions.