Commonly stocked sizes of Service Center inventory by product family:
Billet
- Diameters from 4.00” (102 mm) to 12.00” (305 mm)
- Rectangular stock made to order
Bar
- Diameters from .500” (12.7 mm) to 4.00” (102 mm)
- Rectangular stock made to order
- European Service Centers stock medical-quality 6-4 ELI wire & bar starting at 197” (5 mm) diameter
Coiled Sheet & Strip
- Thicknesses from .012” (.3 mm) to .125” (3.2 mm)
- Widths from 36” (914 mm) to 48” (1219 mm)
- Lengths cut to customer's required size
- Custom slit width coil available upon request
Sheet
- Thicknesses from .012” (.3 mm) to .187” (4.75 mm)
- Widths from 36” (914 mm) to 48” (1219 mm)
- Standard stocked lengths are 96” (USA) & 2 m (Europe)
- Alternate length sheets available upon request
- Custom-sheared widths and lengths available upon request for next-day shipment
Plate
- Thicknesses from .188” (4.78 mm) to 4.00” (102 mm)
- Lengths cut to customer's required size
- Water jet cut shapes made to order for optimized yield and reduced machining costs
Tubing
- Commercially Pure, Industrial Quality, Welded Seam
- Diameters: .750” (19.05 mm) & 1.00” (25.4 mm)
- Wall thicknesses: .035” (.89 mm) & .049” (1.25 mm)
- Alternate sizes made to order