TIMET offers a wide range of support services to save you time and money. These services include:
![]() |
Water Jet Cutting – Multi-head, large-bed water jet machines located in TIMET's U.S. and European service centers produce product in near-net shapes to dramatically reduce raw material and machining costs. Capabilities to a 96" x 288" (2.4 m x 7.3 m) cutting envelope, up to 4" (100mm) thick with cut tolerances as tight as 0.030" (.76 mm). |
![]() |
Sawing – Extensive saw cutting capacity with plate saws for product sizes up to 240" (6 m) long and cut-off saws for product sizes up to 20" (508 mm) diameter or cross-section. Typical cut tolerance of 0.125" (3.18 mm). |
![]() |
Shearing – Next-day service for sheared parts with capacity up to 0.160" (4 mm) thick x 144" (3658 mm) wide and cut tolerances as tight as 0.030" (.76 mm). |
![]() |
Coil Cutting to Length & Slitting – Give TIMET your finished part size and quantity, and we'll customize your sheet size to reduce waste and raw material costs. |
| Machine/Billet Prep – Let TIMET handle your non-critical three-axis machining, allowing you to focus on your high-value core competencies. | |
| |
Machining – TIMET's network of qualified machine shop partners supports your needs for finished machined parts, ready for assembly. |
![]() |
Laser Cutting – Buy near-net shapes to reduce material costs and extra operations. Thickness up to 0.125" (1.2 mm) with tolerances of +/-0.005" (.13 mm). |
![]() |
Forming – TIMET offers both hot and cold forming of sheet and plate. |
| |
Precision Grinding – All service centers offer flat-roll product with tolerances as tight as +/0.001" (.03 mm). |
![]() |
Stocking Programs |